Chemical properties
Property | Value |
---|---|
Aluminio | 1.8 - 2.4 % Show Material materials with Aluminio of 1.8 - 2.4 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.15 - 0.25 % Show Material materials with Carbono of 0.15 - 0.25 % |
Circonio | 0.01 - 0.1 % Show Material materials with Circonio of 0.01 - 0.1 % |
Cobalto | 1 % Show Material materials with Cobalto of 1 % |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % |
Cromo | 24 - 26 % Show Material materials with Cromo of 24 - 26 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 8 - 11 % Show Material materials with Hierro of 8 - 11 % |
Itrio | 0.05 - 0.12 % Show Material materials with Itrio of 0.05 - 0.12 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Níquel | 59 % Show Material materials with Níquel of 59 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Titanio | 0.1 - 0.2 % Show Material materials with Titanio of 0.1 - 0.2 % |