Chemical properties
Property | Value |
---|---|
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Cobalto | 5 % Show Material materials with Cobalto of 5 % |
Cobre | 1 - 2.4 % Show Material materials with Cobre of 1 - 2.4 % |
Cromo | 28 - 31.5 % Show Material materials with Cromo of 28 - 31.5 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Hierro | 13 - 17 % Show Material materials with Hierro of 13 - 17 % |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % |
Molibdeno | 4 - 6 % Show Material materials with Molibdeno of 4 - 6 % |
Niobio | 0.3 - 1.5 % Show Material materials with Niobio of 0.3 - 1.5 % |
Níquel | 36 % Show Material materials with Níquel of 36 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Silicona | 0.8 % Show Material materials with Silicona of 0.8 % |
Wolframio | 1.5 - 4 % Show Material materials with Wolframio of 1.5 - 4 % |