Chemical properties
Property | Value |
---|---|
Aluminio | 1 - 1.7 % Show Material materials with Aluminio of 1 - 1.7 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Cobre | 1 % Show Material materials with Cobre of 1 % |
Cromo | 21 - 25 % Show Material materials with Cromo of 21 - 25 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 20 % Show Material materials with Hierro of 20 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Níquel | 58 - 63 % Show Material materials with Níquel of 58 - 63 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |