Chemical properties
Property | Value |
---|---|
Aluminio | 2.5 - 4 % Show Material materials with Aluminio of 2.5 - 4 % |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.15 % Show Material materials with Carbono of 0.15 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 27 - 31 % Show Material materials with Cromo of 27 - 31 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 2.5 - 6 % Show Material materials with Hierro of 2.5 - 6 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Niobio | 0.5 - 2.5 % Show Material materials with Niobio of 0.5 - 2.5 % |
Níquel | 53 % Show Material materials with Níquel of 53 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Titanio | 1 % Show Material materials with Titanio of 1 % |