Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.35 - 0.5 % Show Material materials with Carbono of 0.35 - 0.5 % |
Cromo | 33 - 39 % Show Material materials with Cromo of 33 - 39 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 7 % Show Material materials with Hierro of 7 % |
Manganeso | 0.5 - 2 % Show Material materials with Manganeso of 0.5 - 2 % |
Niobio | 0.8 - 1.8 % Show Material materials with Niobio of 0.8 - 1.8 % |
Níquel | 42 - 48 % Show Material materials with Níquel of 42 - 48 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Silicona | 0.5 - 2 % Show Material materials with Silicona of 0.5 - 2 % |