Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Cobre | 0.7 - 1.2 % Show Material materials with Cobre of 0.7 - 1.2 % |
Cromo | 23 - 26 % Show Material materials with Cromo of 23 - 26 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 10 - 17 % Show Material materials with Hierro of 10 - 17 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 5 - 7 % Show Material materials with Molibdeno of 5 - 7 % |
Níquel | 47 % Show Material materials with Níquel of 47 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Titanio | 0.7 - 1.5 % Show Material materials with Titanio of 0.7 - 1.5 % |