Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.01 % Show Material materials with Carbono of 0.01 % |
Cobalto | 5 % Show Material materials with Cobalto of 5 % |
Cobre | 1.5 - 2.5 % Show Material materials with Cobre of 1.5 - 2.5 % |
Cromo | 21 - 23.5 % Show Material materials with Cromo of 21 - 23.5 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Hierro | 18 - 21 % Show Material materials with Hierro of 18 - 21 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 6 - 8 % Show Material materials with Molibdeno of 6 - 8 % |
Niobio | 0.5 % Show Material materials with Niobio of 0.5 % |
Níquel | 40 % Show Material materials with Níquel of 40 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Wolframio | 1.5 % Show Material materials with Wolframio of 1.5 % |