Chemical properties
Property | Value |
---|---|
Aluminio | 0.4 - 1 % Show Material materials with Aluminio of 0.4 - 1 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.08 % Show Material materials with Carbono of 0.08 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 14 - 17 % Show Material materials with Cromo of 14 - 17 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 5 - 9 % Show Material materials with Hierro of 5 - 9 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Niobio | 0.7 - 1.2 % Show Material materials with Niobio of 0.7 - 1.2 % |
Níquel | 70 % Show Material materials with Níquel of 70 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Titanio | 2 - 2.7 % Show Material materials with Titanio of 2 - 2.7 % |