Chemical properties
Property | Value |
---|---|
Aluminio | 0.2 - 0.8 % Show Material materials with Aluminio of 0.2 - 0.8 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Boro | 6E-3 % Show Material materials with Boro of 6E-3 % |
Carbono | 0.08 % Show Material materials with Carbono of 0.08 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 17 - 21 % Show Material materials with Cromo of 17 - 21 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 24 % Show Material materials with Hierro of 24 % |
Manganeso | 0.3 % Show Material materials with Manganeso of 0.3 % |
Molibdeno | 2.8 - 3.3 % Show Material materials with Molibdeno of 2.8 - 3.3 % |
Niobio | 4.8 - 5.5 % Show Material materials with Niobio of 4.8 - 5.5 % |
Níquel | 50 - 55 % Show Material materials with Níquel of 50 - 55 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % |
Titanio | 0.7 - 1.1 % Show Material materials with Titanio of 0.7 - 1.1 % |