Chemical properties
Property | Value |
---|---|
Aluminio | 0.2 % Show Material materials with Aluminio of 0.2 % |
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Cobre | 1.5 - 3 % Show Material materials with Cobre of 1.5 - 3 % |
Cromo | 19.5 - 23.5 % Show Material materials with Cromo of 19.5 - 23.5 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 22 % Show Material materials with Hierro of 22 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 2.5 - 3.5 % Show Material materials with Molibdeno of 2.5 - 3.5 % |
Níquel | 38 - 46 % Show Material materials with Níquel of 38 - 46 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Titanio | 0.6 - 1.2 % Show Material materials with Titanio of 0.6 - 1.2 % |