Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.08 % Show Material materials with Carbono of 0.08 % |
Cobalto | 2.5 % Show Material materials with Cobalto of 2.5 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 1 % Show Material materials with Cromo of 1 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 4 - 7 % Show Material materials with Hierro of 4 - 7 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 26 - 30 % Show Material materials with Molibdeno of 26 - 30 % |
Níquel | 55 % Show Material materials with Níquel of 55 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Vanadio | 0.2 - 0.4 % Show Material materials with Vanadio of 0.2 - 0.4 % |
Wolframio | 1 % Show Material materials with Wolframio of 1 % |