Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.02 % Show Material materials with Carbono of 0.02 % |
Cobalto | 1 % Show Material materials with Cobalto of 1 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 1 % Show Material materials with Cromo of 1 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Hierro | 2 % Show Material materials with Hierro of 2 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 26 - 30 % Show Material materials with Molibdeno of 26 - 30 % |
Níquel | 64 % Show Material materials with Níquel of 64 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Titanio | 0.5 % Show Material materials with Titanio of 0.5 % |
Wolframio | 1 % Show Material materials with Wolframio of 1 % |