Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.01 % Show Material materials with Carbono of 0.01 % |
Cobalto | 2.5 % Show Material materials with Cobalto of 2.5 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 20 - 22.5 % Show Material materials with Cromo of 20 - 22.5 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 2 - 6 % Show Material materials with Hierro of 2 - 6 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Molibdeno | 12.5 - 14.5 % Show Material materials with Molibdeno of 12.5 - 14.5 % |
Níquel | 49 % Show Material materials with Níquel of 49 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 0.08 % Show Material materials with Silicona of 0.08 % |
Vanadio | 0.3 % Show Material materials with Vanadio of 0.3 % |
Wolframio | 2.5 - 3.5 % Show Material materials with Wolframio of 2.5 - 3.5 % |