Chemical properties
Property | Value |
---|---|
Aluminio | 0.4 % Show Material materials with Aluminio of 0.4 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Cobalto | 1 % Show Material materials with Cobalto of 1 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 32.25 - 34.25 % Show Material materials with Cromo of 32.25 - 34.25 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 2 % Show Material materials with Hierro of 2 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Molibdeno | 7.6 - 9 % Show Material materials with Molibdeno of 7.6 - 9 % |
Niobio | 0.5 % Show Material materials with Niobio of 0.5 % |
Níquel | 49 % Show Material materials with Níquel of 49 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Silicona | 0.6 % Show Material materials with Silicona of 0.6 % |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % |
Vanadio | 0.2 % Show Material materials with Vanadio of 0.2 % |
Wolframio | 0.6 % Show Material materials with Wolframio of 0.6 % |