Chemical properties
Property | Value |
---|---|
Aluminio | 0.4 % Show Material materials with Aluminio of 0.4 % |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.01 % Show Material materials with Carbono of 0.01 % |
Cobalto | 0.3 % Show Material materials with Cobalto of 0.3 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 20 - 23 % Show Material materials with Cromo of 20 - 23 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 1.5 % Show Material materials with Hierro of 1.5 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Molibdeno | 19 - 21 % Show Material materials with Molibdeno of 19 - 21 % |
Níquel | 52 % Show Material materials with Níquel of 52 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Wolframio | 0.3 % Show Material materials with Wolframio of 0.3 % |