Chemical properties
Property | Value |
---|---|
Aluminio | 0.5 % Show Material materials with Aluminio of 0.5 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.01 % Show Material materials with Carbono of 0.01 % |
Cobalto | 2 % Show Material materials with Cobalto of 2 % |
Cobre | 1.3 - 1.9 % Show Material materials with Cobre of 1.3 - 1.9 % |
Cromo | 22 - 24 % Show Material materials with Cromo of 22 - 24 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 3 % Show Material materials with Hierro of 3 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Molibdeno | 15 - 17 % Show Material materials with Molibdeno of 15 - 17 % |
Níquel | 52 % Show Material materials with Níquel of 52 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 0.08 % Show Material materials with Silicona of 0.08 % |