Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.01 % Show Material materials with Carbono of 0.01 % |
Cobalto | 2 % Show Material materials with Cobalto of 2 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 14 - 18 % Show Material materials with Cromo of 14 - 18 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Hierro | 3 % Show Material materials with Hierro of 3 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 14 - 18 % Show Material materials with Molibdeno of 14 - 18 % |
Níquel | 56 % Show Material materials with Níquel of 56 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 0.08 % Show Material materials with Silicona of 0.08 % |
Titanio | 0.7 % Show Material materials with Titanio of 0.7 % |
Wolframio | 0.5 % Show Material materials with Wolframio of 0.5 % |