Chemical properties
Property | Value |
---|---|
Aluminio | 0.4 % Show Material materials with Aluminio of 0.4 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 20 - 23 % Show Material materials with Cromo of 20 - 23 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 5 % Show Material materials with Hierro of 5 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Molibdeno | 8 - 10 % Show Material materials with Molibdeno of 8 - 10 % |
Niobio | 3 - 4.1 % Show Material materials with Niobio of 3 - 4.1 % |
Níquel | 58 % Show Material materials with Níquel of 58 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Titanio | 0.4 % Show Material materials with Titanio of 0.4 % |