Chemical properties
Property | Value |
---|---|
Aluminio | 0.4 % Show Material materials with Aluminio of 0.4 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Cobalto | 0.2 % Show Material materials with Cobalto of 0.2 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 21 - 23 % Show Material materials with Cromo of 21 - 23 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 2 % Show Material materials with Hierro of 2 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Molibdeno | 9 - 11 % Show Material materials with Molibdeno of 9 - 11 % |
Niobio | 0.2 % Show Material materials with Niobio of 0.2 % |
Níquel | 58 % Show Material materials with Níquel of 58 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Titanio | 0.4 % Show Material materials with Titanio of 0.4 % |
Wolframio | 2 - 4 % Show Material materials with Wolframio of 2 - 4 % |