Chemical properties
Property | Value |
---|---|
Aluminio | 0.8 - 1.5 % Show Material materials with Aluminio of 0.8 - 1.5 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.05 - 0.15 % Show Material materials with Carbono of 0.05 - 0.15 % |
Cobalto | 10 - 15 % Show Material materials with Cobalto of 10 - 15 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 20 - 24 % Show Material materials with Cromo of 20 - 24 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 3 % Show Material materials with Hierro of 3 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 8 - 10 % Show Material materials with Molibdeno of 8 - 10 % |
Níquel | 44 % Show Material materials with Níquel of 44 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Titanio | 0.6 % Show Material materials with Titanio of 0.6 % |
Wolframio | 0.5 % Show Material materials with Wolframio of 0.5 % |