Chemical properties
Property | Value |
---|---|
Aluminio | 1 - 2 % Show Material materials with Aluminio of 1 - 2 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Bismuto | 1E-4 % Show Material materials with Bismuto of 1E-4 % |
Boro | 0.02 % Show Material materials with Boro of 0.02 % |
Carbono | 0.13 % Show Material materials with Carbono of 0.13 % |
Circonio | 0.15 % Show Material materials with Circonio of 0.15 % |
Cobalto | 15 - 18 % Show Material materials with Cobalto of 15 - 18 % |
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % |
Cromo | 18 - 21 % Show Material materials with Cromo of 18 - 21 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 1.5 % Show Material materials with Hierro of 1.5 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Níquel | 50 % Show Material materials with Níquel of 50 % |
Otro | total 0.5., Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Plata | 5E-4 % Show Material materials with Plata of 5E-4 % |
Plomo | 2E-3 % Show Material materials with Plomo of 2E-3 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Titanio | 2 - 3 % Show Material materials with Titanio of 2 - 3 % |