Chemical properties
Property | Value |
---|---|
Aluminio | 0.3 - 0.6 % Show Material materials with Aluminio of 0.3 - 0.6 % |
Azufre | 7E-3 % Show Material materials with Azufre of 7E-3 % |
Bismuto | 1E-4 % Show Material materials with Bismuto of 1E-4 % |
Boro | 5E-3 % Show Material materials with Boro of 5E-3 % |
Carbono | 0.04 - 0.08 % Show Material materials with Carbono of 0.04 - 0.08 % |
Cobalto | 19 - 21 % Show Material materials with Cobalto of 19 - 21 % |
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % |
Cromo | 19 - 21 % Show Material materials with Cromo of 19 - 21 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 0.7 % Show Material materials with Hierro of 0.7 % |
Manganeso | 0.6 % Show Material materials with Manganeso of 0.6 % |
Molibdeno | 5.6 - 6.1 % Show Material materials with Molibdeno of 5.6 - 6.1 % |
Níquel | 47 % Show Material materials with Níquel of 47 % |
Otro | total 0.5., Al + Ti 2.4 - 2.8. Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Plata | 5E-4 % Show Material materials with Plata of 5E-4 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |
Titanio | 1.9 - 2.4 % Show Material materials with Titanio of 1.9 - 2.4 % |