Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.15 % Show Material materials with Carbono of 0.15 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 12 - 17 % Show Material materials with Cromo of 12 - 17 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 12 % Show Material materials with Hierro of 12 % |
Manganeso | 1 - 4.5 % Show Material materials with Manganeso of 1 - 4.5 % |
Molibdeno | 2.5 - 5.5 % Show Material materials with Molibdeno of 2.5 - 5.5 % |
Niobio | 0.5 - 3 % Show Material materials with Niobio of 0.5 - 3 % |
Níquel | 55 % Show Material materials with Níquel of 55 % |
Otro | total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Silicona | 0.8 % Show Material materials with Silicona of 0.8 % |
Wolframio | 1.5 % Show Material materials with Wolframio of 1.5 % |