Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 13 - 17 % Show Material materials with Cromo of 13 - 17 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 10 % Show Material materials with Hierro of 10 % |
Manganeso | 5 - 10 % Show Material materials with Manganeso of 5 - 10 % |
Niobio | 1 - 3.5 % Show Material materials with Niobio of 1 - 3.5 % |
Níquel | 60 % Show Material materials with Níquel of 60 % |
Otro | Ta 0.3. if gefordert, total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Titanio | 1 % Show Material materials with Titanio of 1 % |