Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Cobalto | 2.5 - 3.5 % Show Material materials with Cobalto of 2.5 - 3.5 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 24 - 26 % Show Material materials with Cromo of 24 - 26 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 16 % Show Material materials with Hierro of 16 % |
Manganeso | 1.2 - 2 % Show Material materials with Manganeso of 1.2 - 2 % |
Molibdeno | 2.5 - 3.5 % Show Material materials with Molibdeno of 2.5 - 3.5 % |
Níquel | 44 - 47 % Show Material materials with Níquel of 44 - 47 % |
Otro | total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 0.8 - 1.2 % Show Material materials with Silicona of 0.8 - 1.2 % |
Wolframio | 2.5 - 3.5 % Show Material materials with Wolframio of 2.5 - 3.5 % |