Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.35 - 0.5 % Show Material materials with Carbono of 0.35 - 0.5 % |
Cromo | 27 - 30 % Show Material materials with Cromo of 27 - 30 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 6 % Show Material materials with Hierro of 6 % |
Manganeso | 0.5 - 1.5 % Show Material materials with Manganeso of 0.5 - 1.5 % |
Níquel | 47 - 50 % Show Material materials with Níquel of 47 - 50 % |
Otro | total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 0.5 - 2 % Show Material materials with Silicona of 0.5 - 2 % |
Wolframio | 4 - 5.5 % Show Material materials with Wolframio of 4 - 5.5 % |