Chemical properties
Property | Value |
---|---|
Aluminio | 0.1 % Show Material materials with Aluminio of 0.1 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Cobre | 1.5 - 3 % Show Material materials with Cobre of 1.5 - 3 % |
Cromo | 23 - 27 % Show Material materials with Cromo of 23 - 27 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 30 % Show Material materials with Hierro of 30 % |
Manganeso | 1 - 3 % Show Material materials with Manganeso of 1 - 3 % |
Molibdeno | 3.5 - 7.5 % Show Material materials with Molibdeno of 3.5 - 7.5 % |
Níquel | 37 - 42 % Show Material materials with Níquel of 37 - 42 % |
Otro | total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 0.7 % Show Material materials with Silicona of 0.7 % |
Titanio | 1 % Show Material materials with Titanio of 1 % |