Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.02 % Show Material materials with Carbono of 0.02 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 25 - 27 % Show Material materials with Cromo of 25 - 27 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 1.5 % Show Material materials with Hierro of 1.5 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Molibdeno | 13.5 - 15 % Show Material materials with Molibdeno of 13.5 - 15 % |
Níquel | 55 % Show Material materials with Níquel of 55 % |
Otro | total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt. |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % |