Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 20.5 - 22.5 % Show Material materials with Cromo of 20.5 - 22.5 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 5 % Show Material materials with Hierro of 5 % |
Manganeso | 2.2 % Show Material materials with Manganeso of 2.2 % |
Molibdeno | 8.8 - 10 % Show Material materials with Molibdeno of 8.8 - 10 % |
Niobio | 1 - 2.8 % Show Material materials with Niobio of 1 - 2.8 % |
Níquel | 57 % Show Material materials with Níquel of 57 % |
Otro | total 0.5.ausgenommen Co and Ta, Up to 1 % (mass fraction) of the nickel composition can be present as cobalt., Up to 20 % (mass fraction) of the niobium composition can be replaced by tantalum. |
Silicona | 0.7 % Show Material materials with Silicona of 0.7 % |
Wolframio | 0.5 % Show Material materials with Wolframio of 0.5 % |