General
Property | Value | Condition | Related Standards |
---|---|---|---|
Densidad | 2.65 g/cm³ Show Material materials with Densidad of 2.65 g/cm³ | T6 | EN 1706 |
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Bending Fatigue Strength | 80.0 - 110.0 MPa Show Material materials with Bending Fatigue Strength of 80.0 - 110.0 MPa | T6 | EN 1706 | |
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | ||
Dureza Brinell | 75.0 [-] Show Material materials with Dureza Brinell of 75.0 [-] | T6 | EN 1706 | |
90.0 [-] Show Material materials with Dureza Brinell of 90.0 [-] | T6 | EN 1706 | ||
Módulo de cizallamiento | 2.8 GPa Show Material materials with Módulo de cizallamiento of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | ||
Módulo elástico | 74.0 GPa Show Material materials with Módulo elástico of 74.0 GPa | T6 | EN 1706 | |
Resistencia a la tracción | 220.0 MPa Show Material materials with Resistencia a la tracción of 220.0 MPa | T6 | EN 1706 | |
260.0 MPa Show Material materials with Resistencia a la tracción of 260.0 MPa | T6 | EN 1706 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Calor específico | 910.0 J/(kg·K) Show Material materials with Calor específico of 910.0 J/(kg·K) | T6 | EN 1706 | |
Coeficiente de dilatación térmica | 20 °C | 2.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 1/K | T6 | EN 1706 |
100 °C | 2.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 1/K | T6 | EN 1706 | |
Conductividad térmica | 150.0 - 170.0 W/(m·K) Show Material materials with Conductividad térmica of 150.0 - 170.0 W/(m·K) | T6 | EN 1706 | |
Temperatura de fusión | 550.0 - 600.0 °C Show Material materials with Temperatura de fusión of 550.0 - 600.0 °C | T6 | EN 1706 |
Eléctrico
Property | Value | Condition | Related Standards |
---|---|---|---|
Conductividad eléctrica | 19000000.0 - 25000000.0 S/m Show Material materials with Conductividad eléctrica of 19000000.0 - 25000000.0 S/m | T6 | EN 1706 |
Resistividad eléctrica | 4e-08 - 5.26e-08 Ω·m Show Material materials with Resistividad eléctrica of 4e-08 - 5.26e-08 Ω·m | T6 | EN 1706 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Cobre | 0.05 % Show Material materials with Cobre of 0.05 % | T6 | EN 1706 |
Hierro | 0.50 % Show Material materials with Hierro of 0.50 % | T6 | EN 1706 |
Magnesio | 0.2 - 0.5 % Show Material materials with Magnesio of 0.2 - 0.5 % | T6 | EN 1706 |
Manganeso | 0.001 - 0.4 % Show Material materials with Manganeso of 0.001 - 0.4 % | T6 | EN 1706 |
Silicona | 9.0 - 11.0 % Show Material materials with Silicona of 9.0 - 11.0 % | T6 | EN 1706 |
Titanio | 0.15 % Show Material materials with Titanio of 0.15 % | T6 | EN 1706 |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | T6 | EN 1706 |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not recommended | |
Corrosion properties | general: good | |
General machinability | after thermal treatment: good to acceptable, as cast: good |