General
Property | Value | Condition | Related Standards |
---|---|---|---|
Densidad | 2.75 g/cm³ Show Material materials with Densidad of 2.75 g/cm³ | T64 | EN 1706 |
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Bending Fatigue Strength | 80.0 - 110.0 MPa Show Material materials with Bending Fatigue Strength of 80.0 - 110.0 MPa | T64 | EN 1706 | |
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 2xx.x Series Aluminium | ||
Dureza Brinell | 85.0 [-] Show Material materials with Dureza Brinell of 85.0 [-] | T64 | EN 1706 | |
90.0 [-] Show Material materials with Dureza Brinell of 90.0 [-] | T64 | EN 1706 | ||
Módulo elástico | 72.0 GPa Show Material materials with Módulo elástico of 72.0 GPa | T64 | EN 1706 | |
Resistencia a la tracción | 280.0 MPa Show Material materials with Resistencia a la tracción of 280.0 MPa | T64 | EN 1706 | |
320.0 MPa Show Material materials with Resistencia a la tracción of 320.0 MPa | T64 | EN 1706 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Calor específico | 900.0 J/(kg·K) Show Material materials with Calor específico of 900.0 J/(kg·K) | T64 | EN 1706 | |
Coeficiente de dilatación térmica | 20 °C | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T64 | EN 1706 |
100 °C | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T64 | EN 1706 | |
Conductividad térmica | 120.0 - 150.0 W/(m·K) Show Material materials with Conductividad térmica of 120.0 - 150.0 W/(m·K) | T64 | EN 1706 | |
Temperatura de fusión | 540.0 - 640.0 °C Show Material materials with Temperatura de fusión of 540.0 - 640.0 °C | T64 | EN 1706 |
Eléctrico
Property | Value | Condition | Related Standards |
---|---|---|---|
Conductividad eléctrica | 16000000.0 - 23000000.0 S/m Show Material materials with Conductividad eléctrica of 16000000.0 - 23000000.0 S/m | T64 | EN 1706 |
Resistividad eléctrica | 4.35e-08 - 6.25e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.35e-08 - 6.25e-08 Ω·m | T64 | EN 1706 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Cobre | 4.5 - 5.2 % Show Material materials with Cobre of 4.5 - 5.2 % | T64 | EN 1706 |
Hierro | 0.18 % Show Material materials with Hierro of 0.18 % | T64 | EN 1706 |
Manganeso | 0.001 - 0.5 % Show Material materials with Manganeso of 0.001 - 0.5 % | T64 | EN 1706 |
Silicona | 0.18 % Show Material materials with Silicona of 0.18 % | T64 | EN 1706 |
Titanio | 0.15 % Show Material materials with Titanio of 0.15 % | T64 | EN 1706 |
Zinc | 0.07 % Show Material materials with Zinc of 0.07 % | T64 | EN 1706 |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: acceptable | |
Corrosion properties | general: not sufficient | |
General machinability | as cast: excellent |