General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.4 g/cm³ Show Material materials with Densidad of 8.4 g/cm³ |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 23.0 °C | 120 W/(m·K) Show Material materials with Conductividad térmica of 120 W/(m·K) |
Temperatura de fusión | 890 - 910 °C Show Material materials with Temperatura de fusión of 890 - 910 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 1.50E+7 S/m Show Material materials with Conductividad eléctrica of 1.50E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Cobre | 58 - 62 % Show Material materials with Cobre of 58 - 62 % |
Estaño | 1 % Show Material materials with Estaño of 1 % |
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Manganeso | 0.3 % Show Material materials with Manganeso of 0.3 % |
Otro | Rest Zn, total 0.2 |
Plomo | 0.03 % Show Material materials with Plomo of 0.03 % |
Silicona | 0.1 - 0.5 % Show Material materials with Silicona of 0.1 - 0.5 % |