General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 23.0 °C | 45 W/(m·K) Show Material materials with Conductividad térmica of 45 W/(m·K) |
Temperatura de fusión | 1100 - 1145 °C Show Material materials with Temperatura de fusión of 1100 - 1145 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 5.00E+6 S/m Show Material materials with Conductividad eléctrica of 5.00E+6 S/m |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 1 - 2 % Show Material materials with Hierro of 1 - 2 % |
Manganeso | 0.5 - 1.5 % Show Material materials with Manganeso of 0.5 - 1.5 % |
Níquel | 9 - 11 % Show Material materials with Níquel of 9 - 11 % |
Otro | Rest Cu, total 0.4, Ti can be replaced by Nb |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % |
Titanio | 0.2 - 0.5 % Show Material materials with Titanio of 0.2 - 0.5 % |