General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.7 g/cm³ Show Material materials with Densidad of 7.7 g/cm³ |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 23.0 °C | 65 W/(m·K) Show Material materials with Conductividad térmica of 65 W/(m·K) |
Temperatura de fusión | 1030 - 1040 °C Show Material materials with Temperatura de fusión of 1030 - 1040 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 8.00E+6 S/m Show Material materials with Conductividad eléctrica of 8.00E+6 S/m |
Chemical properties
Property | Value |
---|---|
Aluminio | 7.5 - 9.5 % Show Material materials with Aluminio of 7.5 - 9.5 % |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Níquel | 0.8 % Show Material materials with Níquel of 0.8 % |
Otro | Rest Cu, total 0.4 |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |