General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.5 g/cm³ Show Material materials with Densidad of 7.5 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 380 J/(kg·K) Show Material materials with Calor específico of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Conductividad térmica | 23.0 °C | 20 - 40 W/(m·K) Show Material materials with Conductividad térmica of 20 - 40 W/(m·K) | |
Temperatura de fusión | 1000 - 1040 °C Show Material materials with Temperatura de fusión of 1000 - 1040 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 4.00E+6 - 5.00E+6 S/m Show Material materials with Conductividad eléctrica of 4.00E+6 - 5.00E+6 S/m |
Chemical properties
Property | Value |
---|---|
Aluminio | 6.5 - 8.5 % Show Material materials with Aluminio of 6.5 - 8.5 % |
Hierro | 3 - 4 % Show Material materials with Hierro of 3 - 4 % |
Manganeso | 2.5 % Show Material materials with Manganeso of 2.5 % |
Níquel | 4 - 6 % Show Material materials with Níquel of 4 - 6 % |
Otro | Rest Cu, total 0.5 |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Silicona | 0.7 % Show Material materials with Silicona of 0.7 % |