Chemical properties
Property | Value |
---|---|
Aluminio | 7.3 - 8.8 % Show Material materials with Aluminio of 7.3 - 8.8 % |
Cobre | 82 - 84.5 % Show Material materials with Cobre of 82 - 84.5 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 0.6 % Show Material materials with Hierro of 0.6 % |
Magnesio | 0.04 % Show Material materials with Magnesio of 0.04 % |
Manganeso | 5.3 - 6.5 % Show Material materials with Manganeso of 5.3 - 6.5 % |
Níquel | 1.2 - 1.8 % Show Material materials with Níquel of 1.2 - 1.8 % |
Otro | total 0.4 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 0.05 % Show Material materials with Silicona of 0.05 % |
Zinc | 0.15 % Show Material materials with Zinc of 0.15 % |