General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Calor específico of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Conductividad térmica | 23.0 °C | 220 - 315 W/(m·K) Show Material materials with Conductividad térmica of 220 - 315 W/(m·K) | |
Temperatura de fusión | 1070 - 1080 °C Show Material materials with Temperatura de fusión of 1070 - 1080 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 3.00E+7 - 4.50E+7 S/m Show Material materials with Conductividad eléctrica of 3.00E+7 - 4.50E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Arsénico | 0.05 % Show Material materials with Arsénico of 0.05 % |
Cobre | 99.5 % Show Material materials with Cobre of 99.5 % |
Fósforo | 0.01 - 0.05 % Show Material materials with Fósforo of 0.01 - 0.05 % |
Hierro | 0.05 % Show Material materials with Hierro of 0.05 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Otro | Cu+Ag > 99.5, total 0.1, for gas welding as G-CuAg with P > 0.02%, for inert gas welding P < 0.02% |
Plata | 0.8 - 1.2 % Show Material materials with Plata of 0.8 - 1.2 % |
Plomo | 0.01 % Show Material materials with Plomo of 0.01 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |