Chemical properties
Property | Value |
---|---|
Aluminio | 0.1 % Show Material materials with Aluminio of 0.1 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Magnesio | 0.05 % Show Material materials with Magnesio of 0.05 % |
Manganeso | 1.5 - 3 % Show Material materials with Manganeso of 1.5 - 3 % |
Níquel | 29 - 33 % Show Material materials with Níquel of 29 - 33 % |
Otro | Rest Cu, total 0.6 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 0.05 % Show Material materials with Silicona of 0.05 % |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % |