Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Bismuto | 0.01 % Show Material materials with Bismuto of 0.01 % |
Estaño | 4 - 6 % Show Material materials with Estaño of 4 - 6 % |
Fósforo | 0.05 - 0.1 % Show Material materials with Fósforo of 0.05 - 0.1 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Níquel | 0.2 % Show Material materials with Níquel of 0.2 % |
Otro | total 1.0 |
Plomo | 0.2 % Show Material materials with Plomo of 0.2 % |
Zinc | 0.3 % Show Material materials with Zinc of 0.3 % |