Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % |
Antimonio | 0.5 % Show Material materials with Antimonio of 0.5 % |
Estaño | 7.5 - 9 % Show Material materials with Estaño of 7.5 - 9 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | 0.4 % Show Material materials with Hierro of 0.4 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % |
Otro | total 1.0 |
Plomo | 2 - 4 % Show Material materials with Plomo of 2 - 4 % |
Zinc | 5 - 7 % Show Material materials with Zinc of 5 - 7 % |