Chemical properties
Property | Value |
---|---|
Aluminio | 4.5 - 6 % Show Material materials with Aluminio of 4.5 - 6 % |
Antimonio | 0.1 % Show Material materials with Antimonio of 0.1 % |
Cobre | 63 - 68 % Show Material materials with Cobre of 63 - 68 % |
Estaño | 1 % Show Material materials with Estaño of 1 % |
Hierro | 2 - 4 % Show Material materials with Hierro of 2 - 4 % |
Manganeso | 1.5 - 2.5 % Show Material materials with Manganeso of 1.5 - 2.5 % |
Otro | Rest Zn, total 2.0 |
Plomo | 1 % Show Material materials with Plomo of 1 % |