Chemical properties
Property | Value |
---|---|
Aluminio | 0.7 - 1.5 % Show Material materials with Aluminio of 0.7 - 1.5 % |
Antimonio | 0.1 % Show Material materials with Antimonio of 0.1 % |
Cobre | 57 - 61 % Show Material materials with Cobre of 57 - 61 % |
Estaño | 0.2 - 0.7 % Show Material materials with Estaño of 0.2 - 0.7 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | 0.75 - 1.5 % Show Material materials with Hierro of 0.75 - 1.5 % |
Manganeso | 0.1 - 0.6 % Show Material materials with Manganeso of 0.1 - 0.6 % |
Otro | Rest Zn, total 0.7 |
Plomo | 0.4 % Show Material materials with Plomo of 0.4 % |