Chemical properties
Property | Value |
---|---|
Aluminio | 0.5 - 2 % Show Material materials with Aluminio of 0.5 - 2 % |
Cobre | 56 - 60 % Show Material materials with Cobre of 56 - 60 % |
Estaño | 1.5 % Show Material materials with Estaño of 1.5 % |
Hierro | 1 % Show Material materials with Hierro of 1 % |
Manganeso | 0.5 - 2 % Show Material materials with Manganeso of 0.5 - 2 % |
Níquel | 1 % Show Material materials with Níquel of 1 % |
Otro | Rest Zn, total 5.0 |
Plomo | 1.5 % Show Material materials with Plomo of 1.5 % |