Chemical properties
Property | Value |
---|---|
Aluminio | 6 - 6.4 % Show Material materials with Aluminio of 6 - 6.4 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 0.5 - 0.7 % Show Material materials with Hierro of 0.5 - 0.7 % |
Magnesio | 0.05 % Show Material materials with Magnesio of 0.05 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Níquel | 0.1 % Show Material materials with Níquel of 0.1 % |
Otro | Rest Cu, total 0.80 |
Plomo | 0.03 % Show Material materials with Plomo of 0.03 % |
Silicona | 2 - 2.4 % Show Material materials with Silicona of 2 - 2.4 % |
Zinc | 0.4 % Show Material materials with Zinc of 0.4 % |