General
Property | Value | Comment |
---|---|---|
Densidad | 2.75 - 2.8 g/cm³ Show Material materials with Densidad of 2.75 - 2.8 g/cm³ | Typical for Cast 2xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 2xx.x Series Aluminium | |||
Dureza Brinell | 75.0 [-] Show Material materials with Dureza Brinell of 75.0 [-] | T4 | Pink Sheets, ASTM B108 | Casting | |
Módulo elástico | 72.0 GPa Show Material materials with Módulo elástico of 72.0 GPa | Typical for Cast 2xx.x Series Aluminium | |||
Resistencia a la tracción | 230.0 MPa Show Material materials with Resistencia a la tracción of 230.0 MPa | T4 | Pink Sheets, ASTM B108 | Casting |
Aplicaciones térmicas
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Calor específico | 875.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 875.0 - 963.0 J/(kg·K) | Typical for Cast 2xx.x Series Aluminium | |||
Coeficiente de dilatación térmica | 1.9e-05 - 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9e-05 - 2.3e-05 1/K | Typical for Cast 2xx.x Series Aluminium | |||
Conductividad térmica | 120.0 - 150.0 W/(m·K) Show Material materials with Conductividad térmica of 120.0 - 150.0 W/(m·K) | Typical for Cast 2xx.x Series Aluminium | |||
Temperatura de fusión | 521.0 - 632.0 °C Show Material materials with Temperatura de fusión of 521.0 - 632.0 °C | T4 | Pink Sheets, ASTM B108 | Casting |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 16000000.0 - 23000000.0 S/m Show Material materials with Conductividad eléctrica of 16000000.0 - 23000000.0 S/m | Typical for Cast 2xx.x Series Aluminium |
Resistividad eléctrica | 4.347826086956522e-08 - 6.25e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.347826086956522e-08 - 6.25e-08 Ω·m | Typical for Cast 2xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 4.0 - 5.0 % Show Material materials with Cobre of 4.0 - 5.0 % | T4 | Pink Sheets, ASTM B108 | Casting |
Hierro | 1.20 % Show Material materials with Hierro of 1.20 % | T4 | Pink Sheets, ASTM B108 | Casting |
Magnesio | 0.05 % Show Material materials with Magnesio of 0.05 % | T4 | Pink Sheets, ASTM B108 | Casting |
Manganeso | 0.35 % Show Material materials with Manganeso of 0.35 % | T4 | Pink Sheets, ASTM B108 | Casting |
Níquel | 0.35 % Show Material materials with Níquel of 0.35 % | T4 | Pink Sheets, ASTM B108 | Casting |
Silicona | 2.0 - 3.0 % Show Material materials with Silicona of 2.0 - 3.0 % | T4 | Pink Sheets, ASTM B108 | Casting |
Titanio | 0.25 % Show Material materials with Titanio of 0.25 % | T4 | Pink Sheets, ASTM B108 | Casting |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % | T4 | Pink Sheets, ASTM B108 | Casting |