Chemical properties
Property | Value |
---|---|
Aluminio | 8 - 10 % Show Material materials with Aluminio of 8 - 10 % |
Cobre | 85 - 90 % Show Material materials with Cobre of 85 - 90 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 1 - 4 % Show Material materials with Hierro of 1 - 4 % |
Manganeso | 0.1 - 1 % Show Material materials with Manganeso of 0.1 - 1 % |
Níquel | 0.1 - 1 % Show Material materials with Níquel of 0.1 - 1 % |
Plomo | 0.1 % Show Material materials with Plomo of 0.1 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |