Chemical properties
Property | Value |
---|---|
Aluminio | 6 - 9 % Show Material materials with Aluminio of 6 - 9 % |
Cobre | 71 - 84 % Show Material materials with Cobre of 71 - 84 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 2 - 5 % Show Material materials with Hierro of 2 - 5 % |
Manganeso | 7 - 15 % Show Material materials with Manganeso of 7 - 15 % |
Níquel | 1 - 4 % Show Material materials with Níquel of 1 - 4 % |
Plomo | 0.1 % Show Material materials with Plomo of 0.1 % |