Chemical properties
Property | Value |
---|---|
Aluminio | 5E-3 % Show Material materials with Aluminio of 5E-3 % |
Antimonio | 0.2 % Show Material materials with Antimonio of 0.2 % |
Cobre | 86.5 - 89.5 % Show Material materials with Cobre of 86.5 - 89.5 % |
Estaño | 9 - 11 % Show Material materials with Estaño of 9 - 11 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Níquel | 0.8 % Show Material materials with Níquel of 0.8 % |
Plomo | 1 % Show Material materials with Plomo of 1 % |
Silicona | 5E-3 % Show Material materials with Silicona of 5E-3 % |
Zinc | 1 - 3 % Show Material materials with Zinc of 1 - 3 % |