Property | Value |
---|---|
Aluminio | 0.2 % Show Material materials with Aluminio of 0.2 % |
Antimonio | 2E-3 % Show Material materials with Antimonio of 2E-3 % |
Arsénico | 5E-3 % Show Material materials with Arsénico of 5E-3 % |
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Bismuto | 2E-3 % Show Material materials with Bismuto of 2E-3 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Fósforo | 5E-3 % Show Material materials with Fósforo of 5E-3 % |
Hierro | 0.2 - 0.5 % Show Material materials with Hierro of 0.2 - 0.5 % |
Magnesio | 0.03 % Show Material materials with Magnesio of 0.03 % |
Manganeso | 11.5 - 13.5 % Show Material materials with Manganeso of 11.5 - 13.5 % |
Níquel | 2 - 3.5 % Show Material materials with Níquel of 2 - 3.5 % |
Otro | Rest Cu, total 0.5 |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |