Chemical properties
Property | Value |
---|---|
Aluminio | 10.5 - 11.5 % Show Material materials with Aluminio of 10.5 - 11.5 % |
Antimonio | 0.05 % Show Material materials with Antimonio of 0.05 % |
Arsénico | 0.05 % Show Material materials with Arsénico of 0.05 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Fósforo | 0.1 % Show Material materials with Fósforo of 0.1 % |
Hierro | 5 - 6.5 % Show Material materials with Hierro of 5 - 6.5 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Níquel | 5 - 6.5 % Show Material materials with Níquel of 5 - 6.5 % |
Otro | Rest Cu, total 1.5 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % |
Zinc | 0.6 % Show Material materials with Zinc of 0.6 % |